Skip to content

matbench_v0.1 matbench_mp_gap

Individual Task Leaderboard for matbench_mp_gap

Leaderboard for an individual task. Algorithms shown here may include both general purpose and specialized algorithms (i.e., algorithms which are only valid for a subset of tasks in the benchmark.

Leaderboard

algorithm mean mae std mae mean rmse max max_error
ALIGNN 0.1861 0.0030 0.4635 7.4756
MegNet (kgcnn v2.1.0) 0.1934 0.0087 0.4715 7.8821
Finder_v1.2 structure-based version 0.2193 0.0012 0.4989 7.6676
MODNet (v0.1.12) 0.2199 0.0059 0.4525 7.5685
MODNet (v0.1.10) 0.2199 0.0059 0.4525 7.5685
Finder_v1.2 composition-only version 0.2308 0.0029 0.4837 7.8152
SchNet (kgcnn v2.1.0) 0.2352 0.0034 0.5172 9.1171
CrabNet 0.2655 0.0029 0.5898 7.9829
AMMExpress v2020 0.2824 0.0061 0.5611 6.9105
CGCNN v2019 0.2972 0.0035 0.6771 13.6569
RF-SCM/Magpie 0.3452 0.0033 0.6125 7.0601
Dummy 1.3272 0.0060 1.5989 8.5092

Dataset info

Description

Matbench v0.1 test dataset for predicting DFT PBE band gap from structure. Adapted from Materials Project database. Removed entries having a formation energy (or energy above the convex hull) more than 150meV and those containing noble gases. Retrieved April 2, 2019. For benchmarking w/ nested cross validation, the order of the dataset must be identical to the retrieved data; refer to the Automatminer/Matbench publication for more details.

Number of samples: 106113

Task type: regression

Input type: structure

Dataset columns
  • gap pbe: Target variable. The band gap as calculated by PBE DFT from the Materials Project, in eV.
  • structure: Pymatgen Structure of the material.
Dataset reference

A. Jain*, S.P. Ong*, G. Hautier, W. Chen, W.D. Richards, S. Dacek, S. Cholia, D. Gunter, D. Skinner, G. Ceder, K.A. Persson (*=equal contributions) The Materials Project: A materials genome approach to accelerating materials innovation APL Materials, 2013, 1(1), 011002. doi:10.1063/1.4812323

Metadata

{'bibtex_refs': ['@Article{Dunn2020,\n'
                 'author={Dunn, Alexander\n'
                 'and Wang, Qi\n'
                 'and Ganose, Alex\n'
                 'and Dopp, Daniel\n'
                 'and Jain, Anubhav},\n'
                 'title={Benchmarking materials property prediction methods: '
                 'the Matbench test set and Automatminer reference '
                 'algorithm},\n'
                 'journal={npj Computational Materials},\n'
                 'year={2020},\n'
                 'month={Sep},\n'
                 'day={15},\n'
                 'volume={6},\n'
                 'number={1},\n'
                 'pages={138},\n'
                 'abstract={We present a benchmark test suite and an automated '
                 'machine learning procedure for evaluating supervised machine '
                 'learning (ML) models for predicting properties of inorganic '
                 'bulk materials. The test suite, Matbench, is a set of '
                 '13{\\thinspace}ML tasks that range in size from 312 to 132k '
                 'samples and contain data from 10 density functional '
                 'theory-derived and experimental sources. Tasks include '
                 'predicting optical, thermal, electronic, thermodynamic, '
                 "tensile, and elastic properties given a material's "
                 'composition and/or crystal structure. The reference '
                 'algorithm, Automatminer, is a highly-extensible, fully '
                 'automated ML pipeline for predicting materials properties '
                 'from materials primitives (such as composition and crystal '
                 'structure) without user intervention or hyperparameter '
                 'tuning. We test Automatminer on the Matbench test suite and '
                 'compare its predictive power with state-of-the-art crystal '
                 'graph neural networks and a traditional descriptor-based '
                 'Random Forest model. We find Automatminer achieves the best '
                 'performance on 8 of 13 tasks in the benchmark. We also show '
                 'our test suite is capable of exposing predictive advantages '
                 'of each algorithm---namely, that crystal graph methods '
                 'appear to outperform traditional machine learning methods '
                 'given {\\textasciitilde}104 or greater data points. We '
                 'encourage evaluating materials ML algorithms on the Matbench '
                 'benchmark and comparing them against the latest version of '
                 'Automatminer.},\n'
                 'issn={2057-3960},\n'
                 'doi={10.1038/s41524-020-00406-3},\n'
                 'url={https://doi.org/10.1038/s41524-020-00406-3}\n'
                 '}\n',
                 '@article{Jain2013,\n'
                 'author = {Jain, Anubhav and Ong, Shyue Ping and Hautier, '
                 'Geoffroy and Chen, Wei and Richards, William Davidson and '
                 'Dacek, Stephen and Cholia, Shreyas and Gunter, Dan and '
                 'Skinner, David and Ceder, Gerbrand and Persson, Kristin '
                 'a.},\n'
                 'doi = {10.1063/1.4812323},\n'
                 'issn = {2166532X},\n'
                 'journal = {APL Materials},\n'
                 'number = {1},\n'
                 'pages = {011002},\n'
                 'title = {{The Materials Project: A materials genome approach '
                 'to accelerating materials innovation}},\n'
                 'url = '
                 '{http://link.aip.org/link/AMPADS/v1/i1/p011002/s1\\&Agg=doi},\n'
                 'volume = {1},\n'
                 'year = {2013}\n'
                 '}'],
 'columns': {'gap pbe': 'Target variable. The band gap as calculated by PBE '
                        'DFT from the Materials Project, in eV.',
             'structure': 'Pymatgen Structure of the material.'},
 'description': 'Matbench v0.1 test dataset for predicting DFT PBE band gap '
                'from structure. Adapted from Materials Project database. '
                'Removed entries having a formation energy (or energy above '
                'the convex hull) more than 150meV and those containing noble '
                'gases. Retrieved April 2, 2019. For benchmarking w/ nested '
                'cross validation, the order of the dataset must be identical '
                'to the retrieved data; refer to the Automatminer/Matbench '
                'publication for more details.',
 'file_type': 'json.gz',
 'hash': '58b65746bd88329986ed66031a2ac1369c7c522f7bc9f9081528e07097c2c057',
 'input_type': 'structure',
 'mad': 1.3271449960162496,
 'n_samples': 106113,
 'num_entries': 106113,
 'reference': 'A. Jain*, S.P. Ong*, G. Hautier, W. Chen, W.D. Richards, S. '
              'Dacek, S. Cholia, D. Gunter, D. Skinner, G. Ceder, K.A. Persson '
              '(*=equal contributions)\n'
              'The Materials Project: A materials genome approach to '
              'accelerating materials innovation\n'
              'APL Materials, 2013, 1(1), 011002.\n'
              'doi:10.1063/1.4812323',
 'target': 'gap pbe',
 'task_type': 'regression',
 'unit': 'eV',
 'url': 'https://ml.materialsproject.org/projects/matbench_mp_gap.json.gz'}